Thermal Degradation of Environmentally Friendly Phenolic Resin/Al2O3
In this paper, disc insulators made of Al2O3-filled epoxy resin were surface fluorinated using a F2/N2 mixture (12.5% F2) at 50 C and 0.1 MPa for different durations of 15 min, 30 min and 60 min.Web