crushed the ore and separated it by grain size. The finer-grained material, which was higher in uranium content, was shipped to other mills for chemical processing. Coarser-grained material was stored on-site and later reprocessed at the site through a sulfuric acid batch leach process that was used at the mill from 1964 until 1968.Web